E426(UNE) - Chromium stainless steel. Good workability when hot. Used for applications requiring hardness and corrosion and wear resistance. (Corrosion resistance reduced when not heat treated, heat treated and polished resists rust, diluted nitric acid and mild organic acids). Bad weldability. Similar to AISI 420 steel.
Manufacturing Technology - Ingot
Country - Spain(ES)
- Proprietary Equivalents
- Bestar - BE4034
- Bohler-Uddeholm - N540
- Dirostahl - Diro-X46Cr13
- Dorrenberg - R45
- Grimm Edelstahl - RF40
- Kind & Co - RM13H
- Kind & Co - Coracid420-46
- Lohmann - RF
- Lohmann - LO-R 4034
- Metal Ravne - PK4EX
- Ossenberg - RF4
- Platestahl - PMC145
- Stahlwerk Stahlschmidt - Corronon4
- TES - REMANIT4034
- Thyssen-Krupp - 4034
- Thyssen-Krupp - NIROSTA4034
- Trinec - X45Cr13
- Ugine & Alz - Uginox MA4
- Zapp - K40
- Zapp - ARGESTE 1.4034
NOTE - Approximate composition based on manufacturer's or standard reference information and other alloys in the same reference group is shown.
* - Listed as an equivalent or replacement for alloys in this group.
Knife Steel Chart Mobile Support:
Help & support for the Knife Steel Chart for Android.Help & support for the Knife Steel Chart for iOS.
Thanks, Credits And References